Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 37.0 MPa @# of Cycles 10000 , Temperature 140 °C |
5370 psi @# of Cycles 10000 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Fatigue Strength | 37.0 MPa @# of Cycles 10000 , Temperature 140 °C |
5370 psi @# of Cycles 10000 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |