Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® MD1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco ULTRAFIBRE® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |