Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.00 - 5.00 GPa | 435 - 725 ksi | Compression; ISO 527 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Modulus of Elasticity | 0.210 - 5.00 GPa | 30.5 - 725 ksi | Average value: 2.55 GPa Grade Count:39 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Modulus of Elasticity | 0.700 - 5.00 GPa | 102 - 725 ksi | Average value: 2.51 GPa Grade Count:195 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |