Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.90 - 26.9 GPa | 1000 - 3900 ksi | Average value: 15.3 GPa Grade Count:15 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |