Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 8.10 - 23.0 GPa | 1170 - 3340 ksi | Average value: 10.8 GPa Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 5.00 - 23.0 GPa | 725 - 3340 ksi | Average value: 11.4 GPa Grade Count:36 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Modulus of Elasticity | 2.90 - 23.0 GPa | 420 - 3340 ksi | Average value: 12.2 GPa Grade Count:27 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 8.20 - 23.0 GPa @Temperature 60.0 - 150 °C |
1190 - 3340 ksi @Temperature 140 - 302 °F |
Average value: 14.6 GPa Grade Count:1 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |