Modulus of Elasticity 2.00 - 2.30 GPa
290 - 334 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
Modulus of Elasticity 1.70 - 2.30 GPa
247 - 334 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Modulus of Elasticity 1.70 - 2.30 GPa
247 - 334 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Modulus of Elasticity 1.70 - 2.30 GPa
247 - 334 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Modulus of Elasticity 1.70 - 2.30 GPa
247 - 334 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Modulus of Elasticity 0.140 - 2.30 GPa

@Temperature -40.0 - 150 °C
20.3 - 334 ksi

@Temperature -40.0 - 302 °F
Average value: 1.32 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Modulus of Elasticity 1.24 - 2.30 GPa
180 - 334 ksi
Average value: 1.65 GPa Grade Count:8
Overview of materials for Nylon 12, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 1.20 - 2.30 GPa

@Temperature 60.0 - 90.0 °C
174 - 334 ksi

@Temperature 140 - 194 °F
Average value: 1.67 GPa Grade Count:3