Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 190 - 200 GPa | 27600 - 29000 ksi | Youngs Modulus |
MMCC Al/B4C Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Modulus of Elasticity | 180 - 200 GPa | 26100 - 29000 ksi | Youngs Modulus |
MMCC Al/SiC Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Modulus of Elasticity | 165 - 200 GPa | 23900 - 29000 ksi | |
Special Metals NI-SPAN-C® Alloy 902 A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo.. |
|||
Modulus of Elasticity | 160 - 200 GPa | 23200 - 29000 ksi | |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Modulus of Elasticity | 160 - 200 GPa | 23200 - 29000 ksi | |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Modulus of Elasticity | 100 - 200 GPa | 14500 - 29000 ksi | |
Alliance A-5S Alnico Magnetic Material |
|||
Modulus of Elasticity | 100 - 200 GPa | 14500 - 29000 ksi | |
Alliance A-8S Alnico Magnetic Material |
|||
Modulus of Elasticity | 100 - 200 GPa | 14500 - 29000 ksi | |
Alliance A-6S Alnico Magnetic Material |
|||
Modulus of Elasticity | 100 - 200 GPa | 14500 - 29000 ksi | |
Alliance A-2S Alnico Magnetic Material |