Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.00 - 1.40 GPa @Temperature 60.0 - 120 °C |
145 - 203 ksi @Temperature 140 - 248 °F |
Average value: 1.20 GPa Grade Count:1 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Modulus of Elasticity | 0.0500 - 1.40 GPa @Temperature 50.0 - 100 °C |
7.25 - 203 ksi @Temperature 122 - 212 °F |
Average value: 0.422 GPa Grade Count:5 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 1.40 - 1.40 GPa @Temperature 120 - 120 °C |
203 - 203 ksi @Temperature 248 - 248 °F |
Average value: 1.40 GPa Grade Count:1 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |