Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.60 - 13.8 GPa | 957 - 2000 ksi | Average value: 11.5 GPa Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Modulus of Elasticity | 6.60 - 520 GPa | 957 - 75400 ksi | Average value: 105 GPa Grade Count:59 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 6.60 - 9.40 GPa | 957 - 1360 ksi | Average value: 8.03 GPa Grade Count:10 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 6.60 GPa | 957 ksi | |
Lehmann & Voss LUVOCOM® 1105-7460/BL5019 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Chemical and hydrolysis resistance parts, non flamm.. |
|||
Modulus of Elasticity | 6.60 GPa | 957 ksi | DIN 53 504 |
Dow BETAMATE™ 5103-2 Epoxy BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste.. |
|||
Modulus of Elasticity | 6.60 - 10.9 GPa | 957 - 1580 ksi | Average value: 9.31 GPa Grade Count:20 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |