Mechanical Properties Metric English Comments
Modulus of Elasticity 6.21 GPa
900 ksi
ASTM D638
Technetics Group Amicon™ PEEK 30% Glass Filled  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Modulus of Elasticity 6.21 - 14.5 GPa
900 - 2100 ksi
Average value: 8.50 GPa Grade Count:4
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 6.21 GPa
900 ksi
ASTM D638
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue
Information provided by ITW Devcon
Modulus of Elasticity 6.21 GPa
900 ksi
In Tension; ASTM D638
Devcon Brushable Ceramic - Red, Blue Epoxy
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,..
Modulus of Elasticity 6.21 GPa
900 ksi
In Tension; ASTM D638
Devcon Brushable Ceramic - White Epoxy
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,..
Modulus of Elasticity 6.21 GPa
900 ksi
In Tension; ASTM D638
Devcon Sprayable Ceramic™ Epoxy
Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,..