Polymer Property : Modulus of Elasticity = 566 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.90 - 4.20 GPa
566 - 609 ksi
ISO.178 DN.53452
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
Modulus of Elasticity 3.90 - 4.20 GPa
566 - 609 ksi
ISO.178 DN.53452
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
Modulus of Elasticity 3.90 - 17.0 GPa
566 - 2470 ksi
Average value: 9.07 GPa Grade Count:100
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Modulus of Elasticity 3.90 GPa
566 ksi
Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Highly dimensionally stable at e..
Modulus of Elasticity 3.90 GPa
566 ksi
ISO 527-2
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 3.90 GPa
566 ksi
ISO 178
Addiplast Addilene H 520 M40 Polypropylene Homopolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.