Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.03 GPa | 439 ksi | ASTM D638 |
Plaskolite West Optix® CA-61 Clear UV General Purpose Acrylic Resin General purpose acrylic resin, injection molding and extrusion gradeApplications: A general-purpose acrylic resin designed primarily for injection molding. This resin offers a medium melt flow rate.. |
|||
Modulus of Elasticity | 3.03 GPa | 439 ksi | ASTM D638 |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Modulus of Elasticity | 3.03 GPa | 439 ksi | ASTM D638 |
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Modulus of Elasticity | 3.03 - 4.83 GPa | 439 - 700 ksi | Average value: 4.13 GPa Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |