Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 231 GPa | 33500 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® AS4C Carbon Fiber (12,000 Filaments) Weight/length = 0.800 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® AS4C Carbon Fiber (3000 Filaments) Weight/length = 0.200 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® AS4C Carbon Fiber (6000 Filaments) Weight/length = 0.400 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | In Tension |
Cytec Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | In Tension |
Cytec Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | In Tension |
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | In Tension |
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 231 GPa | 33500 ksi | |
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |