Mechanical Properties Metric English Comments
Modulus of Elasticity 0.207 GPa
30.0 ksi
Secant; ASTM D638
Huntsman PE1501 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa..
Modulus of Elasticity 0.207 GPa
30.0 ksi
Secant; ASTM D638
Huntsman PE1503 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Modulus of Elasticity 0.207 GPa
30.0 ksi
Secant; ASTM D638
Huntsman PE1504 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Modulus of Elasticity 0.207 GPa
30.0 ksi
Secant; ASTM D638
Huntsman PE1507 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Modulus of Elasticity 0.207 GPa

@Temperature -20.0 °C
30.0 ksi

@Temperature -4.00 °F
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Copyright © lookpolymers.com All Rights Reserved