Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.75 GPa | 254 ksi | 50% RH |
Murtfeldt Murylon® 6 Cast Nylon 6 Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia.. |
|||
Modulus of Elasticity | 1.75 GPa | 254 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Modulus of Elasticity | 1.75 GPa | 254 ksi | |
Reliance Industries BIOMER P226 compared to PPInformation provided by Reliance Industries |
|||
Modulus of Elasticity | 1.75 - 3.38 GPa | 254 - 490 ksi | Average value: 2.92 GPa Grade Count:79 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 1.75 GPa | 254 ksi | ISO 527-2 |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 1.75 GPa | 254 ksi | ISO 527 |
DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Conditioned Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Modulus of Elasticity | 1.75 GPa | 254 ksi | ISO R527 |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Modulus of Elasticity | 1.75 GPa @Temperature 100 °C |
254 ksi @Temperature 212 °F |
ISO 527 |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Modulus of Elasticity | 1.75 GPa @Temperature 20.0 °C |
254 ksi @Temperature 68.0 °F |
|
Micropol Isoplas P602 Crosslinkable Polyethylene Information provided by Micropol Limited |