Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.140 GPa | 20.3 ksi | Youngs Modulus |
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled
(discontinued **) Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb. |
|||
Modulus of Elasticity | 0.140 - 2.30 GPa @Temperature -40.0 - 150 °C |
20.3 - 334 ksi @Temperature -40.0 - 302 °F |
Average value: 1.32 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 0.140 - 1.57 GPa | 20.3 - 227 ksi | Average value: 0.441 GPa Grade Count:25 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |