Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0200 - 0.180 GPa | 2.90 - 26.1 ksi | |
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Modulus of Elasticity | 0.0200 - 0.180 GPa | 2.90 - 26.1 ksi | |
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | Youngs Modulus |
3M Dyneon™ Fluorel™ Dipolymer, 35% Carbon Black Filled
(discontinued **) Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | ISO 5527 |
Total Evatane® 28 - 03 HDPE, blown film
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | ISO 5527 |
Total Evatane® 28 - 05 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 120 to 150.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Modulus of Elasticity | 0.0200 - 1.10 GPa | 2.90 - 160 ksi | Average value: 0.678 GPa Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | |
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | DIN EN 826 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | |
AorTech Biomaterials ECSil™ 90A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | |
AorTech Biomaterials ECSil™ 90A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.0200 GPa | 2.90 ksi | DIN EN 826 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |