Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.31 - 15.9 GPa | 190 - 2300 ksi | Average value: 9.89 GPa Grade Count:162 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |