Polymer Property : Modulus of Elasticity = 1540 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 10.6 GPa
1540 ksi
ASTM D638
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
Modulus of Elasticity 10.6 - 17.9 GPa
1540 - 2600 ksi
Average value: 13.3 GPa Grade Count:5
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..