Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.770 GPa | 112 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 50 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Modulus of Elasticity | 0.770 GPa | 112 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Modulus of Elasticity | 0.770 GPa | 112 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Modulus of Elasticity | 0.770 GPa | 112 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Modulus of Elasticity | 0.770 GPa | 112 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |