Mechanical Properties Metric English Comments
Modulus of Elasticity 4.10 - 8.64 GPa
595 - 1250 ksi
Average value: 7.00 GPa Grade Count:5
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..