Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 15.0 - 42.0 GPa @Temperature 60.0 - 150 °C |
2180 - 6090 ksi @Temperature 140 - 302 °F |
Average value: 29.5 GPa Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 0.0370 - 42.0 GPa | 5.37 - 6090 ksi | Average value: 7.22 GPa Grade Count:739 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |