Mechanical Properties Metric English Comments
Modulus of Elasticity 8.10 - 23.0 GPa
1170 - 3340 ksi
Average value: 10.8 GPa Grade Count:32
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 5.00 - 23.0 GPa
725 - 3340 ksi
Average value: 11.4 GPa Grade Count:36
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Modulus of Elasticity 2.90 - 23.0 GPa
420 - 3340 ksi
Average value: 12.2 GPa Grade Count:27
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 8.20 - 23.0 GPa

@Temperature 60.0 - 150 °C
1190 - 3340 ksi

@Temperature 140 - 302 °F
Average value: 14.6 GPa Grade Count:1
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..