Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.620 - 18.6 GPa | 89.9 - 2700 ksi | Average value: 8.21 GPa Grade Count:95 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 9.00 - 18.6 GPa | 1310 - 2700 ksi | Average value: 14.0 GPa Grade Count:26 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Modulus of Elasticity | 7.58 - 18.6 GPa | 1100 - 2700 ksi | Average value: 12.1 GPa Grade Count:79 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |