Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0689 - 1.90 GPa | 10.0 - 275 ksi | Average value: 0.579 GPa Grade Count:25 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 0.500 - 1.90 GPa @Temperature 60.0 - 90.0 °C |
72.5 - 276 ksi @Temperature 140 - 194 °F |
Average value: 1.78 GPa Grade Count:8 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 1.50 - 1.90 GPa @Temperature 60.0 - 90.0 °C |
218 - 276 ksi @Temperature 140 - 194 °F |
Average value: 1.70 GPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Modulus of Elasticity | 0.000517 - 1.90 GPa | 0.0750 - 276 ksi | Average value: 0.0881 GPa Grade Count:27 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Modulus of Elasticity | 0.350 - 1.90 GPa @Temperature 60.0 - 150 °C |
50.8 - 276 ksi @Temperature 140 - 302 °F |
Average value: 0.850 GPa Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | 0.00260 - 1.90 GPa | 0.377 - 276 ksi | Average value: 0.818 GPa Grade Count:8 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 1.10 - 1.90 GPa | 160 - 276 ksi | Average value: 1.64 GPa Grade Count:9 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |