Mechanical Properties Metric English Comments
Modulus of Elasticity 1.00 - 1.40 GPa

@Temperature 60.0 - 120 °C
145 - 203 ksi

@Temperature 140 - 248 °F
Average value: 1.20 GPa Grade Count:1
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Modulus of Elasticity 0.0500 - 1.40 GPa

@Temperature 50.0 - 100 °C
7.25 - 203 ksi

@Temperature 122 - 212 °F
Average value: 0.422 GPa Grade Count:5
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Modulus of Elasticity 1.40 - 1.40 GPa

@Temperature 120 - 120 °C
203 - 203 ksi

@Temperature 248 - 248 °F
Average value: 1.40 GPa Grade Count:1
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..