Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 7.40 - 11.0 GPa | 1070 - 1600 ksi | Average value: 9.35 GPa Grade Count:15 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 7.40 GPa | 1070 ksi | ISO 527-1/-2 |
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Conditioned) Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr.. |