Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 58.0 GPa | 8410 ksi | |
Piezo Kinetics 556 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val.. |
|||
Modulus of Elasticity | >= 58.0 GPa @Temperature 300 °C |
>= 8410 ksi @Temperature 572 °F |
Condition T6 |
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | 58.0 GPa | 8410 ksi | |
Schott F5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 58.0 GPa | 8410 ksi | |
Schott Glass 8652 Sealing Glass Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG. |