Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.30 GPa | 479 ksi | ASTM D638 |
Plaskolite Optix® CA-924 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Good impact strength. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | dry |
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | dry |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | 50% RH |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | ASTM D638 |
Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Good impact strength. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | ISO 527 |
Polycasa Lumina CAST PMMA QUINN CAST lumina has even transmission of light across the whole surface when the sheet is illuminated through its edges. QUINN CAST lumina allows a reduction in final frame dimensions. Perfect for.. |
|||
Modulus of Elasticity | 3.30 - 20.3 GPa | 479 - 2940 ksi | Average value: 6.89 GPa Grade Count:65 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Modulus of Elasticity | 3.30 - 6.30 GPa @Temperature 60.0 - 150 °C |
479 - 914 ksi @Temperature 140 - 302 °F |
Average value: 4.75 GPa Grade Count:1 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | |
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | |
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | |
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | ISO 527 |
GEHR Plastics PMMA Acrylic Polymethylmethacrylate is refractory and shows a good mechanical strength, tensile strength and hardness. PMMA is also scratch resistant and easy to polish. It shows good temperature resistance and .. |
|||
Modulus of Elasticity | 3.30 GPa @Temperature 25.0 °C |
479 ksi @Temperature 77.0 °F |
Storage |
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | ISO 178 |
Addiplast Addinyl B2 1 Flame Retardant Nylon 6 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | dry |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | 50% RH |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Modulus of Elasticity | 3.30 GPa | 479 ksi | ASTM D638 |
Toyobo T-751 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion and impact gradesInformation provided by Toyobo Co., Ltd |
|||
Modulus of Elasticity | 3.30 - 3.40 GPa @Temperature 80.0 - 80.0 °C |
479 - 493 ksi @Temperature 176 - 176 °F |
Average value: 3.37 GPa Grade Count:3 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |