Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 10.6 GPa | 1540 ksi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Modulus of Elasticity | 10.6 - 17.9 GPa | 1540 - 2600 ksi | Average value: 13.3 GPa Grade Count:5 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |