Modulus of Elasticity 0.770 GPa
112 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Modulus of Elasticity 0.770 GPa
112 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Modulus of Elasticity 0.770 GPa
112 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Modulus of Elasticity 0.770 GPa
112 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Modulus of Elasticity 0.770 GPa
112 ksi
(stiffness), ASTM D882
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..