Modulus of Elasticity 0.345 GPa

@Temperature -20.0 °C
50.0 ksi

@Temperature -4.00 °F
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Huntsman PE2065 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: General purpose injection molding resin with good flow characteristicsApplications: Injection molding: lids.FDA Notes: Conforms to FDA regulation 21 CFR 177.1..
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Huntsman PE2067 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: High flow resin, provides excellent gloss and surface characteristics, and minimum cycle time.Applications: Injection molding: lids.FDA Notes: Conforms to FDA..
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Huntsman PE2072 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, gloss, and stiffness.Applications: Injection molding: lids and difficult to fill applications...
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Huntsman PE2075 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, and gloss.Applications: Injection molding: lids and difficult to fill applications.FDA Notes: ..
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Huntsman PE2080 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, and gloss.Applications: Injection molding: lids and difficult to fill applications.FDA Notes: ..
Modulus of Elasticity 0.345 - 45.0 GPa
50.0 - 6530 ksi
Average value: 9.83 GPa Grade Count:74
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Huntsman PE2062 Injection Molding Polyethylene  (discontinued **)