Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 0.268 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.268 GPa
38.9 ksi
Molded Sample 2% Secant Modulus
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili..
Copyright © lookpolymers.com All Rights Reserved