Polymer Property : Modulus of Elasticity = 0.140 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.140 GPa
20.3 ksi
Youngs Modulus
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb.
Modulus of Elasticity 0.140 - 2.30 GPa

@Temperature -40.0 - 150 °C
20.3 - 334 ksi

@Temperature -40.0 - 302 °F
Average value: 1.32 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Modulus of Elasticity 0.140 - 1.57 GPa
20.3 - 227 ksi
Average value: 0.441 GPa Grade Count:25
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..