Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.000986 - 2.10 GPa | 0.143 - 305 ksi | Average value: 0.583 GPa Grade Count:31 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Modulus of Elasticity | 0.000986 GPa | 0.143 ksi | After 7 days at 70°C; ASTM D412 ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |