Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2800 MPa @Temperature 23.0 °C |
406000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
Tensile Creep Modulus, 1 hour | 2800 MPa @Temperature 23.0 °C |
406000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Tensile Creep Modulus, 1 hour | 2800 MPa | 406000 psi | ISO 899 |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Tensile Creep Modulus, 1 hour | 2800 MPa | 406000 psi | ISO 899-1 |
Lanxess Pocan® B 2505 000000 PBT PBT, non-reinforced, injection molding, flame retardant |
|||
Tensile Creep Modulus, 1 hour | 2800 MPa @Temperature 23.0 °C |
406000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
Tensile Creep Modulus, 1 hour | 2800 MPa @Time 3600 sec |
406000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Creep Modulus, 1 hour | 2800 MPa | 406000 psi | ISO 899 |
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |