Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 10000 - 14000 MPa | 1.45e+6 - 2.03e+6 psi | Average value: 11700 MPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Tensile Creep Modulus, 1 hour | 10000 MPa | 1.45e+6 psi | ISO 899-1 |
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber
(discontinued **) PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Tensile Creep Modulus, 1 hour | 10000 MPa | 1.45e+6 psi | ISO 899-1 |
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Tensile Creep Modulus, 1 hour | 10000 MPa | 1.45e+6 psi | ISO 899-1 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Tensile Creep Modulus, 1 hour | 10000 MPa @Time 3600 sec |
1.45e+6 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 10000 MPa @Time 3600 sec |
1.45e+6 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Creep Modulus, 1 hour | 10000 - 11000 MPa | 1.45e+6 - 1.60e+6 psi | Average value: 10500 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |