Polymer Property : Tensile Creep Modulus, 1 hour = 4030 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 3100 - 4030 MPa
450000 - 585000 psi
Average value: 3430 MPa Grade Count:4
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..