Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2800 MPa

@Temperature 23.0 °C
406000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p..
Tensile Creep Modulus, 1 hour 2800 MPa

@Temperature 23.0 °C
406000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov..
Tensile Creep Modulus, 1 hour 2800 MPa
406000 psi
ISO 899
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
Tensile Creep Modulus, 1 hour 2800 MPa
406000 psi
ISO 899-1
Lanxess Pocan® B 2505 000000 PBT
PBT, non-reinforced, injection molding, flame retardant
Tensile Creep Modulus, 1 hour 2800 MPa

@Temperature 23.0 °C
406000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
Tensile Creep Modulus, 1 hour 2800 MPa

@Time 3600 sec
406000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..
Tensile Creep Modulus, 1 hour 2800 MPa
406000 psi
ISO 899
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Conditioned)
Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade.
Copyright © lookpolymers.com All Rights Reserved