Tensile Impact Strength 180 kJ/m²
85.7 ft-lb/in²
Solvay Specialty Polymers Kadel® E-1300 Polyketone  (discontinued **)
High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r..