Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 110 - 280 kJ/m² | 52.3 - 133 ft-lb/in² | Average value: 167 kJ/m² Grade Count:5 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Impact Strength | 110 kJ/m² | 52.3 ft-lb/in² | ASTM D1822 |
Global POM-270 Low Melt Acetal Information provided by Global Polymers Corporation. |
|||
Tensile Impact Strength | 110 kJ/m² | 52.3 ft-lb/in² | Notched, -30°C; ISO 8256 |
Total Finathene® SI 508 HDPE blow molding
(discontinued **) Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weig.. |