Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 72.0 kJ/m² | 34.3 ft-lb/in² | ASTM D1822 |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Impact Strength | 72.0 kJ/m² | 34.3 ft-lb/in² | ASTM D1822 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Impact Strength | 72.0 kJ/m² | 34.3 ft-lb/in² | ASTM D1822 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Impact Strength | 72.0 kJ/m² | 34.3 ft-lb/in² | Average value: 72.0 kJ/m² Grade Count:3 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |