Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 450 kJ/m² | 214 ft-lb/in² | Type S bar; ASTM D1822 |
Chevron Phillips Marlex® C516 HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Outstanding impact resistanceOutstanding creep resistanceExcellent ESCRExcellent chemical resistanceExcellent melt stabilityApplications: 55 gallon drums.. |
|||
Tensile Impact Strength | 450 kJ/m² | 214 ft-lb/in² | At -20°C; ASTM D1822 |
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 450 kJ/m² | 214 ft-lb/in² | At 23°C; ASTM D1822 |
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 450 kJ/m² | 214 ft-lb/in² | ASTM D1822S |
DuPont™ Surlyn® 8320 Ionomer Resin, Sodium Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sod.. |