Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 131 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 134 PC Nonhalogenated. 3.5 MFR. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 221R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 223 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 223S PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 134 PC (Asia Pacific) 3.5 MFR. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not be used for medical applicati.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 143 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Tensile Impact Strength | 546 kJ/m² | 260 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |