Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0148 GPa | 2.15 ksi | ASTM D638 |
Colorite Polymers 9077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
100% Modulus | 0.0148 GPa | 2.15 ksi | ASTM D-638 |
Axiall 19940 Wire & Cable Flexible PVC 105°C rated insulation compound for 600V, 1/64 wall (18 AWG and larger) and 1000V applications. Approved by UL for THWN-2 (8 AWG and larger) and THW-2 in all sizes and colors. UL approved for 94 .. |
|||
100% Modulus | 0.0148 GPa | 2.15 ksi | ASTM D-638 |
Axiall 4420 Flexible PVC High speed TWP wire harness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0148 GPa | 2.15 ksi | ASTM D-638 |
Axiall 8923 Moldings & Extrusions Flexible PVC Non-lead stabilized, migration resistant gasket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0148 GPa | 2.15 ksi | ASTM D-638 |
Axiall 19940-03 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 1/64 wall, 18 AWG and smaller. UL recognized for THHN, THW, THWN, TW. Oil resistant II and VW-1 rated.Information provided by Georgia GulfGeorgia Gulf bec.. |
|||
100% Modulus | 0.0148 GPa | 2.15 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma.. |
|||
100% Modulus | 0.0148 GPa | 2.15 ksi | Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2173 Fluoroelastomer
(discontinued **) Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneLow viscosityProcess targets: compression moldingProprietary incorporated cure technologyExcellent mold flow and mold release ch.. |