Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.009825 GPa | 1.425 ksi | ASTM D638 |
Colorite Polymers 8077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
100% Modulus | 0.009825 GPa | 1.425 ksi | ASTM D-638 |
Axiall 898 Wire & Cable Flexible PVC Non-lead stabilized, flame retardant, non-migratory, 105°C insulation compound recommended for use in non-migratory applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |