Polymer Property : 100% Modulus = 1.375 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.009480 GPa
1.375 ksi
ASTM D638
Colorite Polymers 7577 Non-Phthalate 77 Series Vinyl Compound
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio..
100% Modulus 0.009480 GPa
1.375 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.009480 GPa
1.375 ksi
ASTM D-638
Axiall 18840 Wire & Cable Flexible PVC
Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..