Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00841 GPa | 1.22 ksi | ASTM D412 |
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00841 GPa | 1.22 ksi | ASTM D412 |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00843 GPa | 1.22 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P High Hardness Extruded Profile FormulationNordel® IP 4725P |