Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00448 GPa | 0.650 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D412-97 |
Saint-Gobain Tygon® SE-200 Inert Tubing Formulation Description: Tygon® SE-200: Without sacrificing the flexibility, glass-like clarity or outstanding bend radius for which Tygon® tubing is known, Tygon® Inert Tubing can handle many applic.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D638 |
Colorite Polymers 6500 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D638 |
Colorite Polymers 6507 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D-638 |
Axiall 6704 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeo.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | |
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2180 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2110Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2110Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D-638 |
Axiall 10640 Wire & Cable Flexible PVC Non-lead stabilized general purpose, highly flexible jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | ASTM D-638 |
Axiall 10641 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacket compound designed for good flexibility and good low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2.. |
|||
100% Modulus | 0.00448 GPa | 0.650 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |