Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D412 |
S&E Specialty Polymers GTPE-2203G1 PVC Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-280A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | |
Elastomer Engineering E558 Polyurethane A specially formulated polyester-based urethane for use in abrasion resistance. At use now in mining, grain handling, and gravel conveying applications. Information provided by Elastomer Engineerin.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D412 |
Lubrizol Estane® ALR E77A-V Thermoplastic Polyurethane Type: Estane® ALR E77A-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D638 |
Colorite Polymers 6033 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 8640 Moldings & Extrusions Flexible PVC General purpose extrusion compound for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 8642 Moldings & Extrusions Flexible PVC General purpose, fungus resistant extrusion and molding compound recommended for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 8670 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips and extruded tubing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 3065 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2176 Fluoroelastomer Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneAbility for fast cure cycles with excellent processing safetyMedium viscosityProcess targets: compression and transfer molding, .. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 11600 Wire & Cable Flexible PVC Clear, non-staining speaker wire insulation and general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 16640 Wire & Cable Flexible PVC Matte finish battery booster cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 6702 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2211 Fluoroelastomer Dyneon FC 2211 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The "dry" ingre.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D638 |
Colorite Polymers 6000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D638 |
Colorite Polymers 6742A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D-638 |
Axiall 18650 Moldings & Extrusions Flexible PVC General purpose compound recommended for 105C applications. Well suited for 105C molding and general purpose extrusions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |